12
VISUAL TROUBLESHOOTING
OF PROCESS E-6
Once you have eliminated improper film storage and incorrect exposure as causes of poor-quality transparencies on KODAK
EKTACHROME Film, check for processing problems. These problems include errors in chemical mixing, order of processing
steps, processing temperature, agitation, washing, replenishment, and solution contamination.
A visual check of the processed film is one way to make an initial diagnosis. You can make a more thorough determination of
the cause of processing problems and the corrective action to take by plotting and evaluating your control-strip densities; see
section 13, “Process Monitoring.”
Table 12-1
Troubleshooting from the Appearance of Processed Film
Appearance of Film
Possible Cause
Very High Maximum
Density (very dark
no apparent image)
No Edgeprint
Visible
First developer omitted
Edgeprint
Visible
First developer and color developer reversed
Film not exposed
Dark Overall
Inadequate time or low temperature in first developer
First or color developer diluted or exhausted
Color developer starter added to first developer
Too much first developer starter used
First developer or first and color developers underreplenished
Very Dark (overall or in random areas)
LIght Overall
Bleach or fixer (or both) omitted, reversed, diluted, exhausted, or underreplenished
Too much time or high temperature in first developer
Film fogged by light before processing
First or color developer (or both) too concentrated
First or color developer (or both) overreplenished
First developer starter omitted
First developer contaminated with reversal bath or color developer
First developer contaminated with fixer
Image Very Faint or No Image
(film may show colored streaks)
First developer used twice or color developer omitted
Severe light fog
Overall Density Variation from Batch to Batch
Blue
Inconsistent first-developer time, temperature, agitation, or replenishment
First developer contaminated with fixer
Reversal bath overconcentrated
Too little first developer starter used
Cyan
First-wash temperature too low
Yellow
Color-developer starter added to first developer
Too much first developer starter used
Inadequate bleaching or fixing
Yellow-Red
First developer with color developer starter added
Underreplenishment of first developer or color developer
Low Density Blue; High Density Yellow
Green
Color developer contaminated with fixer
Reversal bath exhausted, diluted, or underreplenished
Film fogged by green safelight
Wash used between color developer and reversal bath
Color developer dilute
Color pH high
Too much Part A in color developer
Overreplenished color developer
A dilute color developer
Color developer mixed using first developer starter
Using KODAK Chemicals, Process E-6 • Z-119 Sixth Edition
12-1
|
Infiniti Network Card WLI CB G300N User Manual
Jaguar Automobile JJM211099101 User Manual
Jensen CD Player CD 472 User Manual
JVC MP3 Player RC EX36S User Manual
JVC VCR HR J281MS User Manual
Jwin Stereo System CD8500 User Manual
KEF Audio Speaker K1157 User Manual
Kenwood Two Way Radio KSGCP401 User Manual
Konica Minolta All in One Printer bizhub C300 User Manual
Konica Minolta Digital Camera DiMAGE G600 User Manual